Company Achievement
Inland achievement:
| Customer Name | Products | Project |
| Baoshan Iron and Steel Group | Incoloy800HT | Rolling mill furnace parts |
| China Shipbuilding Corporation | 254Smo | Ship Engine Parts |
| National Petroleum | Inconel625 | Refinery container fasteners |
| Sinopec | Inconel600 | Petrochemical pipeline flange |
| Harbin Steam Turbine Plant | Incoloy901 | Generator shaft |
Abroad achievement:
Middle East customers: Inconel718, Monel400, Rod, Flange
India customers: Incoloy800H, Pipe
U.S. customers: Inconel718, Inconel625, Flange, Accessories
European customers: Inconel600, Steel pipe, flange