Monel k-500

Monel K-500 Chemical composition:
Alloy
%
Ni
Cu
Al
Ti
Fe
Mn
S
C
Si
Monle K500

Min.

63
27.0
2.30
0.35
 
 
Max.
 
33.0
3.15
0.85
2.0
1.5
0.01
0.25
0.5

Monel K-500 Physical properties :
Density
8.44 g/cm3
Melting point
1315-1350℃

Monel K-500 minimum mechanical properties in the room temperature:
Status
Tensile strength
Rm N/mm2
Yield strength
RP0.2N/mm2
Elongation
A5 %
Monel K500
1100
790
20
 
Alloy K-500 has approximately twice the tensile strength and triple the yield strength of Alloy 400. The strength of Alloy K-500 is maintained to 1200 degrees Fahrenheit, but stays ductile and tough down to temperatures of -400 degrees Fahrenheit. Alloy K-500 also stays non-magnetic to -200 degrees Fahrenheit.
Additional characteristics of Alloy K-500 include outstanding corrosion resistance in a wide range of chemical and marine surroundings, from salts and alkalis, non-oxidizing acids to pure water. Alloy K-500 is non-magnetic and spark resistant. It is also recommended that Alloy K-500 be annealed when it is welded and that any weldments be stress relieved prior to aging.
 
Industries Served:
  • gas & oil extraction
  • chemical processing
  • marine engineering
Shanghai Fengqu Superalloy Co., Ltd.  Tel:+86-21-69155998  
Sales:+86-21-69155989/69151848   Consulting Tel:13817961313 Fax:+86-21-69151848
Add:101#,Boxue Rd, Jiading District, Shanghai,China Zip:201801  E-mail:Sales@superalloy.com.cn