| Product Forms |
Specifications(mm) |
Illustrations |
| Rod & Bar |
Forged Scaled |
Φ50-250,L:1000-4000 |
 |
| Lathed |
Φ60-250,L:800-2500 |
| Hot Rolled |
Φ20-50,L:2000-5000 |
| Cold Drawn |
Φ4-20,L:2000-5000 |
| Wire |
Hot Rolled |
Accepted to delivery in spools. |
 |
| Cold Drawn |
Accepted to delivery in spools. |
| Plate & Sheet |
Hot Rolled |
厚T:4.5~36,宽W:650~2000,长L:1000~4500 |
 |
| Cold Rolled |
厚T:0.8~4.5,宽W:650~1000,长L:800~2200 |
| Pipe & Tube |
Seamless |
外径OD:Φ6~273,壁厚WT:1~30,长L:1000~8000 |
 |
| Welded |
According to your request. |
| Fitting |
Wrought |
Delivery according to ASME B16.9. |
 |
| Forged |
Delivery according to ASME B16.11. |
| Flange |
|
Delivery according to ASME B16.5. |
 |