Invar alloy

Invar 36 Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Co

Mo

P

S

Invar 36

Min.

35

 

Balance

 

 

Max.

38

0.5

0.1

0.06

0.35

1.0

0.5

0.02

0.025


Invar 36 Physical properties:

Density

8.1 g/cm3

Melting point

1430 ℃


Invar 36 Mechanical properties in the room temperature:
Alloy state
Tensile strength
Rm N/mm2
Yield strength
RP0.2N/mm2
Elongation
A5 %
Brinell hardness
 HB
Invar 36
490
240
42
≤200

Characteristic:
36 alloy is a special ultra-low coefficient of heat expansion of low-iron-nickel alloy. One of carbon and manganese element of control is very important. Cold deformation can reduce the coefficient of thermal expansion, in particular within the framework of the heat treatment temperature coefficient of thermal expansion will enable stabilization. Has the following characteristics:
1.Has very low coefficient of heat expansion between the temperature of -250℃ and 200℃.
2.Good toughness and plastic

Metallurgical structure
Invar 36 is the face centered cubic lattice structure

Corrosion resistance
Invar 36 has corrosion resistance in the dry air of room temperature.In other harsh environments, such as the humid air, there may be corrosion (rust).

Applied field
Invar 36 suit for need to apply ultra-low coefficient of heat expansion environment.Typical applications are as follows:
1.Liquefied gas production, storage and transport
2.The measurement and control instruments work temperature lower than 200℃, such as temperature regulating device
3.Metals and other materials use the screw connector bush
4.Bimetal and bimetallic temperature controller
5.Film framework
6.Shadow mask
7.CRP components of the aviation industry temper Die
8.lower than -200℃ the satellite and missile electronic control unit framework
9.The auxiliary tube of the electromagnetic lens in the laser control device

 

Shanghai Fengqu Superalloy Co., Ltd.  Tel:+86-21-69155998  
Sales:+86-21-69155989/69151848   Consulting Tel:13817961313 Fax:+86-21-69151848
Add:101#,Boxue Rd, Jiading District, Shanghai,China Zip:201801  E-mail:Sales@superalloy.com.cn