Alloy |
% |
Ni |
Cr |
Fe |
Nb |
Co |
C |
Mn |
Si |
S |
Cu |
Al |
Ti |
|
Inconel X-750 |
Min. |
|
14 |
5.0 |
0.7 |
|
|
|
|
|
|
0.4 |
2.25 |
|
Max. |
70 |
17 |
9.0 |
1.2 |
1.00 |
0.08 |
1.00 |
0.5 |
0.01 |
0.5 |
1.0 |
2.75 |
Inconel X-750 Physical properties:
|
Density |
8.28 g/cm3 |
|
Melting range |
1393-1427℃ |
Inconel X-750 Alloy m inimum Mechanical properties in the room temperature:
|
Alloy |
Tensile strength |
Yield strength |
Elongation |
Brinell hardness HB |
|
Solution treatment |
1267 |
868 |
25 |
≤400 |
Inconel X-750 Characteristic as below::
Inconel X-750 is a precipitation-hardenable alloy which has been used in applications such as high temperature structural members for gas turbines, jet engine parts, nuclear power plant applications, heat-treating fixtures, forming tools, and extrusion dies. The alloy is highly resistant to chemical corrosion and oxidation and has high stress-rupture strength and low creep rates under high stresses at temperatures up to 1500°F (816°C) after suitable heat treatment.
Inconel X-750 is a precipitation-hardenable alloy which has been used in applications such as high temperature structural members for gas turbines, jet engine parts, nuclear power plant applications, heat-treating fixtures, forming tools, and extrusion dies. The alloy is highly resistant to chemical corrosion and oxidation and has high stress-rupture strength and low creep rates under high stresses at temperatures up to 1500°F (816°C) after suitable heat treatment.
Inconel X-750 Machinability:
Conventional machining techniques used for iron based alloys may be used. This alloy does work-harden during machining and has higher strength and "gumminess" not typical of steels. Heavy duty machining equipment and tooling should be used to minimize chatter or work-hardening of the alloy ahead of the cutting.
Inconel X-750 Corrosion resistance:
Inconel X-750 has excellent resistance to chloride ion stress-corrosion cracking. It exhibits satisfactory resistance to numerous oxidizing environments. The alloy has similar corrosion resistance to alloy 600 in many media.
Incoloy X-750 Application range and field:
- Nuclear reactors
- Gas turbines
- Rocket engines
- Pressure vessels
- Aircraft structures