Inconel 601 Chemaical composition:
Alloy
%
Ni
Cr
Fe
C
Mn
Si
Cu
Al
P
S
601

Min.

58
21
 
 
 
 
 
1.0
 
 
Max.
63
25
balance
0.1
1.5
0.5
1
1.7
0.02
0.015

Inconel 601 Physical properties
Density
8.1g/cm³
Melting point
1320-1370℃

Inconel 601 Alloy m inimum mechanical properties in the room temperature
Alloy state
Tensile strength
Rm N/mm²
Yield strength
R P0. 2N/mm²
Elongation
A 5 %
Brinell hardness
HB
Annealing treatment
650
300
30
-
Solution treatment
600
240
30
≤220

Characteristic as below:
1.Excellent inoxidability in the high temperature.
2.Good resistance to carbonizing.
3.Good inoxidabilitiy in sulfur atmosphere
4.Good mechanical property in both room temperature and high temperature.
5.Good resistance to stress corrosion cracking, 601 have high creep rupture strength since it limits the carbon content and grain size, so recommend to use for above 500℃ environment.
 
Inconel 601 Metallurgical structure:
601 is face-centered cubic lattice structure.
 
Inconel 601 Corrosion resistance
One of the mainly performance of 601 is inexorability in high temperature, even in very inclement conditions. If in the process of heating and cooling cycle, 601 can generate the dense layer of oxide film to get high spalling resistance. 601 have good carbonation resistance. With excellent inoxidability in the high temperature of sulfur atmosphere since it has high chromium and aluminum content.
 
Inconel 601 Application field:
1.The tray,basket and tool clamp in the heat treatment factory.
2.Steel shares at annealing and radiation control, high-speed gas burners, Industrial furnace silk screen.
3.Separate tank of ammonia reforming and catalytic support grid of nitric acid producing.
4.Exhaust system parts
5.Solid waste incinerator's combustion chamber
6.Channel support and soot dealing parts.
7.Detoxification exhaust system components
8.Oxygen re-heater
Shanghai Fengqu Superalloy Co., Ltd.  Tel:+86-21-69155998  
Sales:+86-21-69155989/69151848   Consulting Tel:13817961313 Fax:+86-21-69151848
Add:101#,Boxue Rd, Jiading District, Shanghai,China Zip:201801  E-mail:Sales@superalloy.com.cn