Incoloy 800HT

Incoloy 800HT Chemical composition:
Alloy
%
Ni
Cr
Fe
C
Mn
Si
Cu
S
Al
Ti
800

Min.

30
19
 
 
 
 
 
 
0.15
0.15
Max.
35
23
balance
0.10
1.5
1
0.75
0.015
0.60
0.60
800H

Min.

30
19
 
0.05
 
 
 
 
0.15
0.15
Max.
35
23
balance
0.10
1.5
1
0.75
0.015
0.60
0.60
800HT

Min.

30
19
 
0.06
 
 
 
 
0.15
0.15
Max.
35
23
balance
0.10
1.5
1
0.75
0.015
0.60
0.60
AI+Ti: 0.85-1.20

Incoloy 800HT Physical properties:
Density
8.0 g/cm³
Melting point
1350-1400 ℃

Incoloy 800HT Alloy m inimum mechanical properties in the room temperature
Alloy
Tensile strength
Rm N/mm²
Yield strength
R P0. 2N/mm²
Elongation
A 5 %
800
500
210
35
800H
450
180
35
800H Characteristic as below:
1.Excellent corrosion resistance in the high temperature at 500℃ in the water medium.
2.Good stress corrosion resistance property.
3.Good machining
 
Incoloy 800HT Metallurgical structure:
800H is face-centered cubic lattice structure. very low carbon centent and increased Ti:C rate
improve the stability of the structure, anti-allergy , and anti-intergranular corrosion. Low temperature annealing of 950℃ ensure the fine grain structure.
 
Incoloy 800HT Corrosion resistance:
800H can not be corroded in many kinds of media. Its high nickel content made it have good stress corrosion resistance cracking property in the water corrosion condition.High Chromium content made it can better resist pitting and crevice corrosion cracking. This alloy can resist nitric acid and organic acid corrosion, but it is not so fine in the sulfuric acid and hydrochloric acid.
800H not only good corrosion resistance in both oxidation and non-oxidizing salt, maybe a little pitting in halide, but also very good corrosion resistance property in the mixture of water,smoke, steam,air and carbon dioxide.
 
Incoloy 800HT Application range and field:
1.Nitrate condenser---Corrosion resistance of nitrc acid
2.Steam heating pipes--Very good mechanical property
3.Heat up element tube--Very good mechanical property
 
For the application of up to 500℃ enviornment, alloy supply state change to annealing.
Shanghai Fengqu Superalloy Co., Ltd.  Tel:+86-21-69155998  
Sales:+86-21-69155989/69151848   Consulting Tel:13817961313 Fax:+86-21-69151848
Add:101#,Boxue Rd, Jiading District, Shanghai,China Zip:201801  E-mail:Sales@superalloy.com.cn