Hastelloy C-276

Hastelloy C-276 Chemical composition
Alloy
%
Ni
Cr
Mo
Fe
W
Co
C
Mn
Si
V
P
S
C

Min.

balance
14.5
15
4
3
 
 
 
 
 
 
 
Max.
16.5
17
7
4.5
2.5
0.08
1
1
0.35
0.04
0.03
C276
Min.
balance
14.5
15
4
3
 
 
 
 
 
 
 
Max.
16.5
17
7
4.5
2.5
0.01
1
0.08
0.35
0.04
0.03

Hastelloy C-276 Physical properties:
Density
8.9 g/cm³
Melting point
1325-1370 ℃

Hastelloy C-276 Alloy m inimum mechanical properties in the room temperature
Alloy state
Tensile strength
Rm N/mm²
Yield strength
R P0. 2N/mm²
Elongation
A 5 %
C /C276
690
283
40

Characteristic as below
1.Excellent corrosion resistance to most of corrosion media in oxidation and reduction environments.
2.Excellent resist pitting, crevice corrosion and stress corrosion cracking performance.
 
Hastelloy C-276 Metallurgical structure
C276 is face-centered cubic lattice structure.
 
Hastelloy C-276 Corrosion resistance
C276 alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant. High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make it corrosion resistance better.C276 is one of a few material that can resist the corrosion of most chlorine, hypochlorite and chlorine dioxide, this alloy have prominent corrosion resistance to high concentration chlorate( iron chloride and copper chloride).

Hastelloy C-276 Application field:
C276 is widely used in the chemical field and petrifaction field, such as the element of chloride organic and catalyze system.This material especially suit for high temperature environment, impure inorganic acid and organic acid (such as formic acid and acetic acid), sea-water corrosion environment.
 
Hastelloy C-276 Other application field:
1. The digester and bleacher in the use of paper pulp and paper making industry.
2.Absorption tower, re-heater and fan in the FGD system.
3. The equipment and parts in the use of acidic gas environments.
4. Acetic acid and anhydride reaction generator
5. Sulfur acid cooling
6.MDI
7.Manufacture and processing of impure phosphoric acid.
Shanghai Fengqu Superalloy Co., Ltd.  Tel:+86-21-69155998  
Sales:+86-21-69155989/69151848   Consulting Tel:13817961313 Fax:+86-21-69151848
Add:101#,Boxue Rd, Jiading District, Shanghai,China Zip:201801  E-mail:Sales@superalloy.com.cn