A-286

A-286 Chemical composition:
Alloy
%
Ni
Cr
Mo
B
Fe
Al
Ti
C
Mn
Si
V
S
A-286

Min.

24
13.5
1.0
0.001
 
 
1.9
0.1
 
Max.
27
16
1.5
0.01
Balance
0.35
2.35
0.08
2.0
1.0
0.5
0.03

A-286 Physical properties:
Density
7.93 g/cm3
Melting point
1364-1424℃

A-286 minimum mechanical properties in the room temperature:
Status
Tensile strength
Rm N/mm2
Yield strength
RP0.2N/mm2
Elongation
A5 %
A-286
950
680
28
 
An alloy that is precipitation hardenable for high mechanical properties. The alloy maintains good strength and oxidation resistance at temperatures up to about 1300°F (700°C). The alloy’s high strength and excellent fabrication characteristics make it useful for various components of aircraft and industrial gas turbines. Applications include blades, vanes, shafts, tail cones, afterburners, springs, and fasteners. This alloy is also used for automotive applications.
Shanghai Fengqu Superalloy Co., Ltd.  Tel:+86-21-69155998  
Sales:+86-21-69155989/69151848   Consulting Tel:13817961313 Fax:+86-21-69151848
Add:101#,Boxue Rd, Jiading District, Shanghai,China Zip:201801  E-mail:Sales@superalloy.com.cn