返回首页 Shanghai Fengqu Superalloy Co., Ltd.
Search
中    文
English
Home About us Products Services News Contacts us  

690-80A

Inconel 690 (UNS N06690) Nimonic 80A (UNS N07080)
Summary

Inconel 690 is a high-chromium nickel alloy having excellent resistance to many corrosive aqueous media and high-temperature atmospheres. The alloy's high chromium content gives it excellent resistance to aqueous corrosion by oxidizing acids (especially nitric acid) and salts, and to sulfidation at high-temperatures. In addition to its corrosion
resistance, alloy 690 has high strength, good metallurgical stability, and favorable fabrication characteristics.

A nickel-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile and creep-rupture properties at temperatures to ℃.Used for gasturbine components (blades, rings, and discs), bolts, tube supports in nuclear steam generators, die-casting inserts and cores, and exhaust valves in internal-combustion engines.
Standard
Product Forms
Pipe, tube, plate, round bar and forging stock.

Sheet, round bar, flat bar, forging stock, hexagon, wire, extruded section and plate.
Limiting Chemical Composition, %
  Min. Max.   Min. Max.   Min. Max.
Ni 58.0   Cu   0.5 C   0.05
Cr 27.0 31.0 Co   Si   0.5
Fe 7.0 11.0 Al     P    
Mo     Ti     S   0.015
W     Mn   0.5 N    
  Min. Max.   Min. Max.   Min. Max.
Ni Remainder Cu   0.2 C   0.1
Cr 18.0 21.0 Co 2.0 Si   1.0
Fe   3.0 Al 0.5 1.8 P    
Mo     Ti 1.8 2.7 S    
Zr     Mn   1.0 B    
Physical
Constants
Density,g/cm3   8.19
Melting Range,℃   1343-1377
Density,g/cm3   8.19
Melting Range,℃   1320-1365
Typical
Mechanical
Properties


(Precipitation Hardened)    
Rupture Strength (1000h) ksi Mpa
1100°F/595°C 94 650
1200°F/650°C 73 500
1300°F/705°C 51 350
1400°F/760°C 32 220
1500°F/815°C 16 110
Shanghai Fengqu Superalloy Co., Ltd.  Tel:+86-21-69155998  
Sales:+86-21-69155989/69151848   Consulting Tel:13817961313 Fax:+86-21-69151848
Add:101#,Boxue Rd, Jiading District, Shanghai,China Zip:201801  E-mail:Sales@superalloy.com.cn