Incoloy 926

Incoloy 926 Chemical composition:

Alloy

%

Ni

Cr

Fe

C

Mn

Si

Cu

Mo

N

P

S

 

926

Min.

24

19

Balance

0.5

6.0

0.15

 

Max.

26

21

0.02

2

0.5

1.5

7.0

0.25

0.03

0.01

 


Incoloy 926 Physical properties:

Density

8.1 g/cm3

Melting point

1320-1390 ℃


Incoloy 926 Alloy Minimum Mechanical properties in the room temperature:
Alloy state
Tensile strength
Rm N/mm2
Yield strength
RP0.2N/mm2
Elongation
A5 %
926
650
295
35
 
Incoloy 926 Characteristic:
1.It has high resistance to pitting and crevice corrosion when in Halide and H2S contained acid media.
2.In practice, effective in resistance of chloride stress corrosion cracking.
3.A variety of corrosion have good corrosion resistance capability in the normal oxidation and restore environment.
4.Upgrade mechanical properties than Cronifer 1925 LC-Alloy 904 L.
5. Alloys has Improved the stability of metallurgical compared to a range of 18% of the nickel content alloys.
6.With a certification of applied in manufacturing-related  pressure vessel (VdTUV-196~400℃ and ASME )

Metallurgical structure
926 is face-centered cubic lattice structure.

Corrosion resistance
926 is an austenitic stainless steel alloy has a similar chemical composition with 904L alloy, its nitrogen content is 0.2%, molybdenum content is 6.5%. Molybdenum and nitrogen content significantly increased the resistance of pitting and crevice corrosion  in the halide media.Meantime, nickel and nitrogen not only ensures the stability of metallographical, but also reduce separating intergranular trend in the thermal process or welding process better than the nitrogen content of nickel alloy. 926 has particular corrosion resistance in the chloride ions medium due to the excellent local corrosion resistance and 25% nickel alloy content.A variety of experiments in the 10000-70000ppm of Chloride concentration, PH 5-6, 50-68℃ operating temperature of the slurry of limestone FGD system show that, after a 1-2 year trial period, 926 alloy without pitting and crevice corrosion.926 in other chemical media also has good corrosion resistance in the high temperature and high concentration of media, including sulfuric acid, phosphoric acid, acid gas, sea water, salt and organic acids.926 is the material that choosed for BAM directory Chapter 6 of "dangerous goods storage and transportation containers norms"  by  Berlin, Germany's national Institute for Materials Research and Testing (BAM) . In addition, in order to have the best corrosion resistance only when the material is in the right state of metallurgy and guarantee clean conditions.

Application field:
Alloy 926 is a multipurpose material can be applied in many industrial:
1. Fire system, water purification system, marine engineering and hydraulic piping perfusion system
2. The pipeline, joint, air systems in the acidic gas production
3. Evaporator, the heat exchanger, filter, mixer, etc. in the phosphate production
4.Power plants condensation and pipe system in the use of sewage water to cool water
5. The use of acidic organic catalyst chlorinated derivatives production
6. The production of cellulose pulp bleacher                                              
7. Polished bar in the orrosive oil wells
8. Hose system in the ocean engineering                                                   
9. Flue gas desulphurization system components
10. Sulfuric acid condensation and separation system                              
11. Crystalline salt concentration and the evaporator
12. Transport of corrosive chemicals containers                                        